Farashin ASTM A283 T91 P91 P22 A355 P9 P11 4130 42CrMo 15CrMo Alloy Carbon Karfe Bututu
Takaitaccen Bayani:
42CrMo alloy bututu maras kyau shine ƙarfe mai ƙarfi mai ƙarfi tare da ƙarfi mai ƙarfi da tauri, mai ƙarfi mai ƙarfi, babu ƙarancin zafin jiki, da ƙaramin nakasawa yayin kashewa.Bayan quenching da tempering, 42CrMo gami da bututu maras kyau yana da iyakar gajiya da juriya mai yawa, tasirin tasiri mai kyau a ƙananan zafin jiki, da ƙarfi mai ƙarfi da ƙarfin juriya a babban zafin jiki.Ana amfani da quenching surface bayan quenching da tempering a matsayin tsarin maganin zafi don 42CrMo gami da bututu marasa ƙarfi.
Mun dage kan ka'idar haɓakawa na 'High high quality, Ingantacciyar, ikhlasi da tsarin aiki na ƙasa zuwa ƙasa' don ba ku babban taimako na aiki don farashi mai arha ASTM A283 T91 P91 P22 A355 P9 P11 4130 42CrMo 15CrMo Alloy Carbon Karfe Bututu, Muna da zurfin haɗin gwiwa tare da daruruwan masana'antu kusa da kasar Sin.Abubuwan da muke gabatarwa zasu iya dacewa da kira daban-daban don.Zaba mu, kuma ba za mu sa ku yi nadama!
Mun dage kan ka'idar haɓakawa na 'High high quality, Ingantacciyar, ikhlasi da tsarin aiki na ƙasa zuwa ƙasa' don ba ku babban taimako na sarrafawaAlloy Karfe bututu da Alloy sumul bututu, Shekaru masu yawa na ƙwarewar aiki, mun fahimci mahimmancin samar da samfurori masu kyau da mafita da kuma mafi kyawun tallace-tallace da sabis na tallace-tallace.Yawancin matsalolin da ke tsakanin masu kaya da abokan ciniki suna faruwa ne saboda rashin kyawun sadarwa.A al'adance, masu samar da kayayyaki na iya yin shakkar tambayar abubuwan da ba su fahimta ba.Mun rushe duk waɗannan shingen don tabbatar da samun abin da kuke so zuwa matakin da kuke tsammani, lokacin da kuke so.lokacin bayarwa da sauri kuma samfurin da kuke so shine Ma'aunin mu.
Ba shi da wani bayyanannen tashin hankali, ƙananan nakasawa a lokacin quenching, iyakar gajiya mai yawa da juriya masu yawa bayan quenching da jin zafi.42CrMo gami da bututu maras kyau yana da tasirin tasiri mai kyau a ƙananan zafin jiki da ƙarfi mai ƙarfi da ƙarfin juriya a babban zafin jiki.Ana amfani da quenching surface bayan quenching da tempering a matsayin tsarin maganin zafi don 42CrMo gami da bututu marasa ƙarfi.
Alloy na musamman karfe:41Cr4,25CrMo4,30CrMo4,34CrMo4,42CrMo4
OD: 20-660mm WT: 2.3-100mm L: 5.8M, 6M, 11.8M, 12M ko kowane tsayi da aka ƙayyade.
Aikace-aikace: Machining, Janar injiniya, crane hannu, Bushes, Silinda Daban-daban, Conveyor Rolls, m Shafts, m sassa da aka gyara, Kwaya, Zobba, da dai sauransu
Aikace-aikace na 42CrMo gami da bututu maras kyau: ƙarfe na musamman da ake amfani da shi don gadoji shine “42CrMo”, ƙarfe na musamman don ginshiƙan mota shine “42CrMo”, kuma ƙarfe na musamman don tasoshin matsa lamba shine “42CrMo”.Irin wannan ƙarfe yana inganta kayan aikin ƙarfe ta hanyar daidaita abun ciki na carbon (c).Saboda haka, bisa ga abun ciki na carbon, irin wannan karfe za a iya raba zuwa: low carbon karfe - da carbon abun ciki ne kullum kasa da 0.25%, kamar 10 da 20 karfe;Matsakaicin carbon karfe - abun cikin carbon gabaɗaya tsakanin 0.25 da 0.60%, kamar 35 da 45 karfe;High carbon karfe - da carbon abun ciki ne kullum fi 0.60%.Gabaɗaya ba a amfani da irin wannan ƙarfe don yin bututun ƙarfe.
Aikace-aikace na yau da kullun
Ya dace da yin manyan gyare-gyaren filastik masu girma da matsakaici masu buƙatar takamaiman ƙarfi da tauri.
Karfe daraja | C | Si | Mn | P | S | Cr | Mo | Ni | ||||||
Sunan karfe | Lambar karfe | min. | max. | max. | min. | max. | max. | max. | min. | max. | min. | max. | min. | max. |
41Cr4 | 1.7035 | 0,38 | 0,45 | 0,40 | 0,60 | 0,90 | 0,035 | 0,035 | 0,90 | 1,20 | - | - | - | - |
25CrMo4 | 1.7218 | 0,22 | 0,29 | 0,40 | 0,60 | 0,90 | 0,035 | 0,035 | 0,90 | 1,20 | 0,15 | 0,30 | - | - |
30CrMo4 | 1.7216 | 0,27 | 0,34 | 0,35 | 0,35 | 0,60 | 0,035 | 0,035 | 0,80 | 1,15 | 0,15 | 0,30 | - | - |
34CrMo4 | 1.7220 | 0,30 | 0,37 | 0,40 | 0,60 | 0,90 | 0,035 | 0,035 | 0,90 | 1,20 | 0,15 | 0,30 | - | - |
42CrMo4 | 1.7225 | 0,38 | 0,45 | 0,40 | 0,60 | 0,90 | 0,035 | 0,035 | 0,90 | 1,20 | 0,15 | 0,30 | - | - |
a Duba kuma 7.1. | ||||||||||||||
b<0.25% Ku. |
Karfe daraja | Ƙananan kaddarorin juzu'i | ||||||||||||||||
Sunan karfe | Lambar karfe | Ƙarfin Haɓaka (ReH) MPa | Ƙarfin ƙarfi (RM) MPa | Tsawaita A% | |||||||||||||
Don T a mm | Don T a mm | Don T a mm | |||||||||||||||
T≤8 | 8 t≤20 | 20 | T≤50 | 50 | T≤80 | T≤8 | 8 t≤20 | 20 | T≤50 | 50 | T≤80 | T≤8 | 8 t≤20 | 20 | T≤50 | 50 | T≤80 | ||||||
l | t | l | t | l | t | l | t | ||||||||||
41Cr4 | 1.7035 | 800 | 660 | 560 | - | 1000 | 900 | 800 | - | 11 | 9 | 12 | 10 | 14 | 12 | - | - |
25CrMo4 | 1.7218 | 700 | 600 | 450 | 400 | 900 | 800 | 700 | 650 | 12 | 10 | 14 | 12 | 15 | 13 | 16 | 14 |
30CrMo4 | 1.7216 | 750 | 630 | 520 | 480 | 950 | 850 | 750 | 700 | 12 | 10 | 13 | 11 | 14 | 12 | 15 | 13 |
34CrMo4 | 1.7220 | 800 | 650 | 550 | 500 | 1000 | 900 | 800 | 750 | 11 | 9 | 12 | 10 | 14 | 12 | 15 | 13 |
42CrMo4 | 1.7225 | 900 | 750 | 650 | 550 | 1100 | 1000 | 900 | 800 | 10 | 8 | 11 | 9 | 12 | 10 | 13 | 11 |
NOTE l = mai tsayi, t = juye. |
Haƙuri na Tsawon Tsawon Su:
Lokacin da Tsawon yayi daidai 6000mm, Haƙuri 0/+10
Lokacin 6 000 <L = 12 000, Haƙuri 0/+15
Lokacin> 12 000, Haƙuri 0/+ ta yarjejeniya
Ƙayyadaddun tsari da kaddarorin jiki na 42CrMo karfe bututu
42CrMo karfe bututu, carbon abun ciki: 0.38 ~ 0.45%, silicon: 0.17 ~ 0.37%, manganese: 0.50 ~ 0.80%.
42CrMo karfe bututu nasa ne na matsananci-high ƙarfi karfe, tare da babban ƙarfi da taurin, mai kyau hardenability, babu wani fili tempering brittleness, high gajiya iyaka da mahara tasiri juriya bayan quenching da tempering jiyya, da kuma mai kyau low-zazzabi tasiri tauri.
Karfe ya dace da kera manyan gyare-gyaren filastik masu girma da matsakaici waɗanda ke buƙatar takamaiman ƙarfi da ƙarfi.Madaidaicin ma'auni na ƙungiyar ƙasa da ƙasa: 42CrMo4 yayi daidai da alamar Jafananci: scm440 yayi daidai da alamar Jamusanci: 42CrMo4 kusan daidai da alamar Amurka: halaye 4140 da iyakokin aikace-aikacen: babban ƙarfi, ƙarfin ƙarfi, tauri mai kyau, ƙaramin nakasawa yayin kashewa, ƙarfi mai ƙarfi da ƙarfi. ƙarfin juriya a babban zafin jiki.Ana amfani dashi don kera ƙirƙira tare da ƙarfi mafi girma kuma mafi girma quenching da tempering giciye-sashe fiye da 35CrMo karfe, kamar manyan kaya don locomotive gogayya, watsa kaya na supercharger, raya axle, haɗa sanda da kuma bazara matsa tare da babban kaya, rawar soja hadin gwiwa da kuma kayan aikin kamun kifi na mai mai zurfin rijiyar ƙasa da 2000m, da mold don injin lanƙwasa.
Sulfur s: abun ciki da aka yarda da shi ≤ 0.035%
Phosphorus P: abun ciki da aka halatta ≤ 0.035%
Chromium (CR): 0.90 ~ 1.20%
Nickel Ni: abun ciki da aka halatta ≤ 0.030%
Copper Cu: abun ciki da aka halatta ≤ 0.030%
Molybdenum (MO): 0.15 ~ 0.25%
Danniya mai izini na 42CrMo
42CrMo halatta danniya 186 ~ 310 / MPa, yawan amfanin ƙasa 930 σ S / MPa, 42CrMo yana da babban ƙarfi, hardenability, mai kyau tauri, kananan nakasawa a lokacin quenching, da kuma high creep ƙarfi da jimiri ƙarfi a high zazzabi.Ana amfani da bututun ƙarfe na 42CrMo don kera ƙirƙira tare da ƙarfi mafi girma da yanki mafi girma da zafin jiki fiye da karfe 35CrMo.
1) Matsayi mai mahimmanci (kimanin): AC1 = 730 ° C, AC3 = 800 ° C, Ms = 310 ° C.
2) Matsakaicin fadada layin layi: zafin jiki 20 ~ 100 ° C / 20 ~ 200 ° C / 20 ~ 300 ° C / 20 ~ 400 ° C / 20 ~ 500 ° C / 20 ~ 600 ° C, madaidaicin haɓakar haɓakawa: 11.1 × 10K /12.1 × 10K/12.9 × 10K/13.5 × 10K/13.9 × 10K14.1 × 10K.
3) Na roba modulus: zafin jiki 20 ° C / 300 ° C / 400 ° C / 500 ° C / 600 ° C, na roba modulus 210000mpa / 185000mpa / 175000mpa / 165000mpa / 15500mpa
Bayanin aiki mai zafi
The dumama zafin jiki ne 1150 ~ 1200 ° C, da farawa zafin jiki ne 1130 ~ 1180 ° C, da kuma karshen zafin jiki ne> 850 ° C, φ> 50mm, jinkirin sanyaya.
Daidaita ƙayyadaddun ƙayyadaddun bayanai
Matsakaicin zafin jiki na yau da kullun shine 850 ~ 900 ° C, kuma tanderun yana sanyaya iska.
Ƙayyadaddun yanayin zafi mai girma
Yanayin zafin jiki shine 680 ~ 700 ° C, kuma tanderun yana sanyaya iska.
Quenching da tempering ƙayyadaddun bayanai
Preheating zazzabi 680 ~ 700 ° C, quenching zafin jiki 840 ~ 880 ° C, mai sanyaya, tempering zazzabi 580 ° C, ruwa sanyaya ko man sanyaya, taurin ≤ 217hbw.
Ƙididdiga don ƙarfafa subcritical da ƙarfafawa
Quenching zafin jiki 900 ° C, zafin jiki na 560 ° C, taurin (37 ± 1) HRC
Ƙayyadewa don quenching induction da tempering
Quenching zafin jiki 900 ° C, tempering zazzabi 150 ~ 180 ° C, taurin 54 ~ 60HRC.
Bayanin aiki mai zafi
The dumama zafin jiki ne 1150 ~ 1200 ° C, da farawa zafin jiki ne 1130 ~ 1180 ° C, da kuma karshen zafin jiki ne> 850 ° C, φ> 50mm, jinkirin sanyaya.
Daidaita ƙayyadaddun ƙayyadaddun bayanai
Matsakaicin zafin jiki na yau da kullun shine 850 ~ 900 ° C, kuma tanderun yana sanyaya iska.
Ƙayyadaddun yanayin zafi mai girma
Yanayin zafin jiki shine 680 ~ 700 ° C, kuma tanderun yana sanyaya iska.
Quenching da tempering ƙayyadaddun bayanai
Preheating zazzabi 680 ~ 700 ° C, quenching zafin jiki 840 ~ 880 ° C, mai sanyaya, tempering zazzabi 580 ° C, ruwa sanyaya ko man sanyaya, taurin ≤ 217hbw.
Ƙididdiga don ƙarfafa subcritical da ƙarfafawa
Quenching zafin jiki 900 ° C, zafin jiki na 560 ° C, taurin (37 ± 1) HRC
Ƙayyadewa don quenching induction da tempering
Quenching zafin jiki 900 ° C, tempering zazzabi 150 ~ 180 ° C, taurin 54 ~ 60HRC.
Mun dage kan ka'idar haɓakawa na 'High high quality, Ingantacciyar, ikhlasi da tsarin aiki na ƙasa zuwa ƙasa' don ba ku babban taimako na aiki don farashi mai arha ASTM A283 T91 P91 P22 A355 P9 P11 4130 42CrMo 15CrMo Alloy Karfe , Muna da zurfin hadin gwiwa tare da daruruwan masana'antu kusa da kasar Sin.Abubuwan da muke gabatarwa zasu iya dacewa da kira daban-daban don.Zaba mu, kuma ba za mu sa ku yi nadama!
Farashin mai arha na bututun ƙarfe na ƙarfe na ƙarfe da bututu mara nauyi, Shekaru da yawa na ƙwarewar aiki, mun fahimci mahimmancin samar da samfuran inganci da mafita da mafi kyawun sabis na siyarwa da bayan-tallace-tallace.Yawancin matsalolin da ke tsakanin masu kaya da abokan ciniki suna faruwa ne saboda rashin kyawun sadarwa.A al'adance, masu samar da kayayyaki na iya yin shakkar tambayar abubuwan da ba su fahimta ba.Mun rushe duk waɗannan shingen don tabbatar da samun abin da kuke so zuwa matakin da kuke tsammani, lokacin da kuke so.lokacin bayarwa da sauri kuma samfurin da kuke so shine Ma'aunin mu.